Fractographic analysis of co-bonded carbon fiber reinforced composites joints subjected to mode I delamination

  • Nubia Nale Alves da Silveira
  • , Rita Sales
  • , Camila Brito
  • , Geraldo Candido
  • , Maurício V. Donadon

Research output: Contribution to conferencePaperpeer-review