Skip to main navigation Skip to search Skip to main content

Fractographic analysis of the hygrothermal effect in co-bonded and secondary bonded joints under Mode II delamination loading

  • Nubia Nale Alves da Silveira (Corresponding Author)
  • , Rita Sales
  • , Geraldo Candido
  • , Maurício V. Donadon

Research output: Contribution to journal › Article › Academic › peer-review

1 Downloads (Pure)
Original languageEnglish
Article number102508
JournalInternational journal of adhesion and adhesives
Volume98
DOIs
Publication statusPublished - Apr 2020
Externally publishedYes

UN SDGs

This output contributes to the following UN Sustainable Development Goals (SDGs)

  1. SDG 9 - Industry, Innovation, and Infrastructure
    SDG 9 Industry, Innovation, and Infrastructure

Keywords

  • Composites
  • Surface Roughness
  • Microscopy

Cite this