Preparation of La0.3Sr0.7CoO3-δ perovskite by thermal decomposition of metal-EDTA complexes

René H.E. van Doorn, Henk Kruidhof, Arian Nijmeijer, Louis Winnubst, Anthony J. Burggraaf

Research output: Contribution to journalArticleAcademicpeer-review

65 Citations (Scopus)
189 Downloads (Pure)

Abstract

Perovskite powders of La0.3Sr0.7CoO3-δ were prepared by the thermal decomposition of precursor complexes derived from nitrate solutions using ethylenediaminetetraacetic acid (EDTA) as a complexing agent. The calcination temperature is 920 °C. Powders thus obtained have a low carbon contamination. Dense ceramics with a relative density of about 96% have been prepared after sintering at 1150 °C.
Original languageEnglish
Pages (from-to)2109-2112
Number of pages4
JournalJournal of materials chemistry
Volume8
Issue number9
DOIs
Publication statusPublished - 1998

Fingerprint

Dive into the research topics of 'Preparation of La0.3Sr0.7CoO3-δ perovskite by thermal decomposition of metal-EDTA complexes'. Together they form a unique fingerprint.